Raw bauxite and titania with molar ratio of Al2O3 : TiO2 as 1.2 : 1 were mixed with varying amounts of SiC. The compacted powder was sintered at different temperatures in the range 1 00-1500°. Magnitude of sintering and properties of the sintered compacted mass were found to be influenced by the SiC additive.